title = "AlxTayOz Mixture Coatings Prepared Using Atomic Layer Deposition for Corrosion Protection of Steel",
keywords = "ALD, Coatings, Corrosion, Low Alloy Steel, Mixtures, Oxides, OXIDE THIN-FILMS, PLASMA ELECTROLYTIC OXIDATION, CARBON-STEEL, ELECTROCHEMICAL CHARACTERIZATION, DIELECTRIC APPLICATIONS, STAINLESS-STEEL, EPITAXY GROWTH, RESISTANCE, BEHAVIOR, POLARIZATION, 116 Chemical sciences",