Atomic Layer Deposition and Lithium-ion Batteries: Studies on new materials and reactions for battery development

Research output: ThesisDoctoral Thesis

Original languageEnglish
Place of PublicationHelsinki
Publisher
Print ISBNs978-951-51-3253-6
Electronic ISBNs978-951-51-3254-3
Publication statusPublished - 2017
MoE publication typeG5 Doctoral dissertation (article)

Fields of Science

  • 116 Chemical sciences
  • ATOMIC LAYER DEPOSITION
  • MATERIALS SCIENCE
  • Thin films
  • LITHIUM-ION BATTERY