Atomic Layer Deposition of Ti x Fe2-x O3 Photoanodes and Photocurrent Response Optimization Using the Response Surface Methodology

Research output: Contribution to journalArticleScientificpeer-review

Original languageEnglish
JournalACS Omega
Volume10
Issue number14
Pages (from-to)14522-14535
Number of pages14
ISSN2470-1343
DOIs
Publication statusPublished - 5 Apr 2025
MoE publication typeA1 Journal article-refereed

Fields of Science

  • Doped hematite nanostructures
  • Thin-films
  • Hydrogen-production
  • Photoelectrocatalysis
  • Precursors
  • 116 Chemical sciences

Cite this