Atomic Layer Deposition on Pharmaceuticals

Tommi Kääriäinen, Jaana Katriina Hautala, Pekka Hoppu, Marja-Liisa Kääriäinen, Anne Juppo, David Cameron, Steven George

Research output: Chapter in Book/Report/Conference proceedingConference contributionScientificpeer-review

Original languageEnglish
Title of host publicationProceedings of the12th International Baltic ALD Conference, Helsinki, Finland.
Publication date2014
Publication statusPublished - 2014
MoE publication typeA4 Article in conference proceedings
EventBaltic ALD 2014 - Helsinki, Finland
Duration: 12 May 201413 May 2014
Conference number: 12

Fields of Science

  • 317 Pharmacy
  • 116 Chemical sciences

Cite this

Kääriäinen, T., Hautala, J. K., Hoppu, P., Kääriäinen, M-L., Juppo, A., Cameron, D., & George, S. (2014). Atomic Layer Deposition on Pharmaceuticals. In Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.
Kääriäinen, Tommi ; Hautala, Jaana Katriina ; Hoppu, Pekka ; Kääriäinen, Marja-Liisa ; Juppo, Anne ; Cameron, David ; George, Steven. / Atomic Layer Deposition on Pharmaceuticals. Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.. 2014.
@inproceedings{027b8cc661ac40efa6f3b3b21e30b3c5,
title = "Atomic Layer Deposition on Pharmaceuticals",
keywords = "317 Pharmacy, 116 Chemical sciences",
author = "Tommi K{\"a}{\"a}ri{\"a}inen and Hautala, {Jaana Katriina} and Pekka Hoppu and Marja-Liisa K{\"a}{\"a}ri{\"a}inen and Anne Juppo and David Cameron and Steven George",
note = "Volume: Proceeding volume:",
year = "2014",
language = "English",
booktitle = "Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.",

}

Kääriäinen, T, Hautala, JK, Hoppu, P, Kääriäinen, M-L, Juppo, A, Cameron, D & George, S 2014, Atomic Layer Deposition on Pharmaceuticals. in Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.. Baltic ALD 2014, Helsinki, Finland, 12/05/2014.

Atomic Layer Deposition on Pharmaceuticals. / Kääriäinen, Tommi; Hautala, Jaana Katriina; Hoppu, Pekka; Kääriäinen, Marja-Liisa; Juppo, Anne; Cameron, David; George, Steven.

Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.. 2014.

Research output: Chapter in Book/Report/Conference proceedingConference contributionScientificpeer-review

TY - GEN

T1 - Atomic Layer Deposition on Pharmaceuticals

AU - Kääriäinen, Tommi

AU - Hautala, Jaana Katriina

AU - Hoppu, Pekka

AU - Kääriäinen, Marja-Liisa

AU - Juppo, Anne

AU - Cameron, David

AU - George, Steven

N1 - Volume: Proceeding volume:

PY - 2014

Y1 - 2014

KW - 317 Pharmacy

KW - 116 Chemical sciences

M3 - Conference contribution

BT - Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.

ER -

Kääriäinen T, Hautala JK, Hoppu P, Kääriäinen M-L, Juppo A, Cameron D et al. Atomic Layer Deposition on Pharmaceuticals. In Proceedings of the12th International Baltic ALD Conference, Helsinki, Finland.. 2014