Low-Temperature Atomic Layer Deposition of Cobalt Oxide as an Effective Catalyst for Photoelectrochemical Water-Splitting Devices

Jiyeon Kim, Tomi Iivonen, Jani Hämäläinen, Marianna Kemell, Kristoffer Meinander, Kenichiro Mizohata, Lidong Wang, Jyrki Räisänen, Radim Beranek, Markku Leskelä, Anjana Devi

Research output: Contribution to journalArticleScientificpeer-review

Original languageEnglish
JournalChemistry of Materials
Volume29
Issue number14
Pages (from-to)5796-5805
Number of pages10
ISSN0897-4756
DOIs
Publication statusPublished - 25 Jul 2017
MoE publication typeA1 Journal article-refereed

Fields of Science

  • 116 Chemical sciences

Cite this

@article{31ec4c06003949108c3c6c72946a485d,
title = "Low-Temperature Atomic Layer Deposition of Cobalt Oxide as an Effective Catalyst for Photoelectrochemical Water-Splitting Devices",
keywords = "116 Chemical sciences",
author = "Jiyeon Kim and Tomi Iivonen and Jani H{\"a}m{\"a}l{\"a}inen and Marianna Kemell and Kristoffer Meinander and Kenichiro Mizohata and Lidong Wang and Jyrki R{\"a}is{\"a}nen and Radim Beranek and Markku Leskel{\"a} and Anjana Devi",
year = "2017",
month = "7",
day = "25",
doi = "10.1021/acs.chemmater.6b05346",
language = "English",
volume = "29",
pages = "5796--5805",
journal = "Chemistry of Materials",
issn = "0897-4756",
publisher = "American Chemical Society Journals",
number = "14",

}

Low-Temperature Atomic Layer Deposition of Cobalt Oxide as an Effective Catalyst for Photoelectrochemical Water-Splitting Devices. / Kim, Jiyeon; Iivonen, Tomi; Hämäläinen, Jani; Kemell, Marianna; Meinander, Kristoffer; Mizohata, Kenichiro; Wang, Lidong; Räisänen, Jyrki; Beranek, Radim; Leskelä, Markku; Devi, Anjana.

In: Chemistry of Materials, Vol. 29, No. 14, 25.07.2017, p. 5796-5805.

Research output: Contribution to journalArticleScientificpeer-review

TY - JOUR

T1 - Low-Temperature Atomic Layer Deposition of Cobalt Oxide as an Effective Catalyst for Photoelectrochemical Water-Splitting Devices

AU - Kim, Jiyeon

AU - Iivonen, Tomi

AU - Hämäläinen, Jani

AU - Kemell, Marianna

AU - Meinander, Kristoffer

AU - Mizohata, Kenichiro

AU - Wang, Lidong

AU - Räisänen, Jyrki

AU - Beranek, Radim

AU - Leskelä, Markku

AU - Devi, Anjana

PY - 2017/7/25

Y1 - 2017/7/25

KW - 116 Chemical sciences

U2 - 10.1021/acs.chemmater.6b05346

DO - 10.1021/acs.chemmater.6b05346

M3 - Article

VL - 29

SP - 5796

EP - 5805

JO - Chemistry of Materials

JF - Chemistry of Materials

SN - 0897-4756

IS - 14

ER -