Atomic Layer Deposition as key enabler of scalable and stable perovskite solar cells

Projekt: Finlands Akademi: Akademiprojektsbidrag

Projektinformation

Beskrivning (abstrakt)

We will develop new preparation methods for thin film materials needed in halide perovskite solar cells. Our aim is to find solutions the two major issues that currently hamper the development of the otherwise promising halide perovskite technology. The issues are instability of the halide perovskites and the lack of scalable preparation methods. Our approach relies on atomic layer deposition (ALD), a unique method that enables the deposition of uniform films on large areas. The work will be done at the department of chemistry, University of Helsinki. The project will provide information on the effects of preparation conditions on film properties. The new methods will be applicable also to other devices such as LEDs. In the long term, the methods developed here can promote the transition to sustainable energy production.
StatusPågående
Gällande start-/slutdatum01/09/202031/08/2024

Finansiering

  • SUOMEN AKATEMIA Vähäkylä Leena: 500 280,00 €