@article{576addd8ffb345e7b7acd64f8efd2bd8,
title = "Atomic Layer Deposition of Ti x Fe2-x O3 Photoanodes and Photocurrent Response Optimization Using the Response Surface Methodology",
keywords = "Doped hematite nanostructures, Thin-films, Hydrogen-production, Photoelectrocatalysis, Precursors, 116 Chemical sciences",
author = "Anjan Deb and Anton Vihervaara and Georgi Popov and Mykhailo Chundak and Abdelaal, \{Ahmed O.\} and Santos, \{Hugo L. S.\} and Heikkila, \{Mikko J.\} and Marianna Kemell and Camargo, \{Pedro H. C.\} and Mikko Ritala and Matti Putkonen",
year = "2025",
month = apr,
day = "5",
doi = "10.1021/acsomega.5c01360",
language = "English",
volume = "10",
pages = "14522--14535",
journal = "ACS Omega",
issn = "2470-1343",
publisher = "American Chemical Society",
number = "14",
}