Integrated atomic layer deposition and chemical vapor reaction for the preparation of metal organic framework coatings for solid-phase microextraction Arrow

Forskningsoutput: TidskriftsbidragArtikelVetenskapligPeer review

Originalspråkengelska
TidskriftAnalytica Chimica Acta
Volym1024
Sidor (från-till)93-100
Antal sidor8
ISSN0003-2670
DOI
StatusPublicerad - 18 sep 2018
MoE-publikationstypA1 Tidskriftsartikel-refererad

Vetenskapsgrenar

  • 116 Kemi

Citera det här

@article{a5f2d3490d4d4b858ed84337506c8721,
title = "Integrated atomic layer deposition and chemical vapor reaction for the preparation of metal organic framework coatings for solid-phase microextraction Arrow",
keywords = "Atomic layer deposition, Chemical vapor reaction, Metal organic frameworks, Solid phase microextraction Arrow, Gas chromatography-mass spectrometry, THIN-FILMS, PHENOLIC-COMPOUNDS, RESPONSE-SURFACE METHODOLOGY, ADSORPTION, OF-THE-ART, CHROMATOGRAPHY-MASS-SPECTROMETRY, WASTE-WATER, OPTIMIZATION, WATER SAMPLES, IONIC LIQUIDS, 116 Chemical sciences",
author = "Hangzhen Lan and Salmi, {Leo D.} and Tuukka R{\"o}nkk{\"o} and Jevgeni Parshintsev and Matti Jussila and Kari Hartonen and Marianna Kemell and Marja-Liisa Riekkola",
year = "2018",
month = "9",
day = "18",
doi = "10.1016/j.aca.2018.04.033",
language = "English",
volume = "1024",
pages = "93--100",
journal = "Analytica Chimica Acta",
issn = "0003-2670",
publisher = "Elsevier Scientific Publ. Co",

}

TY - JOUR

T1 - Integrated atomic layer deposition and chemical vapor reaction for the preparation of metal organic framework coatings for solid-phase microextraction Arrow

AU - Lan, Hangzhen

AU - Salmi, Leo D.

AU - Rönkkö, Tuukka

AU - Parshintsev, Jevgeni

AU - Jussila, Matti

AU - Hartonen, Kari

AU - Kemell, Marianna

AU - Riekkola, Marja-Liisa

PY - 2018/9/18

Y1 - 2018/9/18

KW - Atomic layer deposition

KW - Chemical vapor reaction

KW - Metal organic frameworks

KW - Solid phase microextraction Arrow

KW - Gas chromatography-mass spectrometry

KW - THIN-FILMS

KW - PHENOLIC-COMPOUNDS

KW - RESPONSE-SURFACE METHODOLOGY

KW - ADSORPTION

KW - OF-THE-ART

KW - CHROMATOGRAPHY-MASS-SPECTROMETRY

KW - WASTE-WATER

KW - OPTIMIZATION

KW - WATER SAMPLES

KW - IONIC LIQUIDS

KW - 116 Chemical sciences

U2 - 10.1016/j.aca.2018.04.033

DO - 10.1016/j.aca.2018.04.033

M3 - Article

VL - 1024

SP - 93

EP - 100

JO - Analytica Chimica Acta

JF - Analytica Chimica Acta

SN - 0003-2670

ER -